Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 24.0 MPa @Temperature 750 °C, Time 3.60e+7 sec |
3480 psi @Temperature 1380 °F, Time 10000 hour |
|
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Rupture Strength | 24.0 MPa @Temperature 750 °C, Time 3.60e+7 sec |
3480 psi @Temperature 1380 °F, Time 10000 hour |
|
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Rupture Strength | 24.0 MPa @Temperature 850 °C, Time 3.60e+7 sec |
3480 psi @Temperature 1560 °F, Time 10000 hour |
Stress Rupture |
AFE Technologies Cronite 25Cr/12Ni No. HR7 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |