Rupture Strength 27.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
3920 psi

@Temperature 1470 °F,
Time 10000 hour
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Rupture Strength 27.0 MPa

@Temperature 750 °C,
Time 3.60e+7 sec
3920 psi

@Temperature 1380 °F,
Time 10000 hour
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..