Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 300 MPa @Temperature 704 °C, Time 1.44e+6 sec |
43500 psi @Temperature 1300 °F, Time 400 hour |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |