Mechanical Properties Metric English Comments
Rupture Strength 48.0 MPa

@Temperature 700 °C,
Time 3.60e+7 sec
6960 psi

@Temperature 1290 °F,
Time 10000 hour
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Rupture Strength 48.0 MPa

@Temperature 927 °C,
Time 3.60e+6 sec
6960 psi

@Temperature 1700 °F,
Time 1000 hour
Plate
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Rupture Strength 48.0 MPa

@Temperature 800 °C,
Time 3.60e+7 sec
6960 psi

@Temperature 1470 °F,
Time 10000 hour
Stress Rupture
AFE Technologies Cronite 657 Nickel Alloy Castings
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..