Mechanical Properties Metric English Comments
Rupture Strength 3.447 MPa

@Temperature 871 °C,
Time 3.60e+6 sec
500.0 psi

@Temperature 1600 °F,
Time 1000 hour
Crucible Steel 446 Chromium Steel
Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi..