Mechanical Properties Metric English Comments
Rupture Strength 550 MPa

@Temperature 650 °C,
Time 36000 sec
79800 psi

@Temperature 1200 °F,
Time 10.0 hour
Initial Stress
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Rupture Strength 550 MPa

@Temperature 704 °C,
Time 3.60e+6 sec
79800 psi

@Temperature 1300 °F,
Time 1000 hour
Special Metals UDIMET® alloy R41 Ni-Cr Alloy
UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al..
Rupture Strength 550 MPa

@Temperature 732 °C,
Time 720000 sec
79800 psi

@Temperature 1350 °F,
Time 200 hour
Crucible Compaction Metals P/M Low Carbon Astroloy, Supersolvus
P/M Low Carbon Astroloy is often the superalloy of choice when applications require greater ductility along with substantial strength levels. When HIP and heat treatment above the solvus temperatur..