Polymer Property : Rupture Strength = 60000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 413.7 MPa

@Temperature 32.2 °C,
Time 3.60e+6 sec
60000 psi

@Temperature 90.0 °F,
Time 1000 hour
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Rupture Strength 413.7 MPa

@Temperature 32.2 °C,
Time 3.60e+6 sec
60000 psi

@Temperature 90.0 °F,
Time 1000 hour
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Rupture Strength 413.7 MPa

@Temperature 32.2 °C,
Time 3.60e+6 sec
60000 psi

@Temperature 90.0 °F,
Time 1000 hour
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..