Polymer Property : Rupture Strength = 6380 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 44.0 MPa

@Temperature 927 °C,
Time 3.60e+6 sec
6380 psi

@Temperature 1700 °F,
Time 1000 hour
Special Metals UDIMET® alloy L-605 Co-Cr-W-Ni Alloy
UDIMET® alloy L-605 (UNS R30605) is a solid solution strengthened cobalt-chromium-tungsten-nickel alloy with excellent high-temperature strength and excellent oxidation resistance to 2000°F (1093°..