Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 689 MPa @Temperature 593 °C, Time 1.44e+6 sec |
100000 psi @Temperature 1100 °F, Time 400 hour |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |
|||
Rupture Strength | 689 MPa @Temperature 538 °C, Time 3.96e+7 sec |
100000 psi @Temperature 1000 °F, Time 11000 hour |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |