Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 5.516 MPa @Temperature 871 °C, Time 3.60e+6 sec |
800.0 psi @Temperature 1600 °F, Time 1000 hour |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |