Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 63.0 MPa @Temperature 700 °C, Time 3.60e+7 sec |
9140 psi @Temperature 1290 °F, Time 10000 hour |
|
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Rupture Strength | 63.0 MPa @Temperature 700 °C, Time 3.60e+7 sec |
9140 psi @Temperature 1290 °F, Time 10000 hour |
|
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |