Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 13.6 J @Temperature 22.8 °C |
10.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |