Mechanical Properties Metric English Comments
Dart Drop, Total Energy 12.0 J

@Temperature -40.0 °C
8.85 ft-lb

@Temperature -40.0 °F
ASTM D3763
SABIC Innovative Plastics NORYL PVX516 PPE
PREVEX* PVX516 resin is a high flow, non FR grade, 110 C HDT