Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 16.3 J @Temperature 22.8 °C |
12.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil LD 506.07 Compounding and molding resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Dart Drop, Total Energy | 16.3 J @Temperature 22.8 °C |
12.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Dart Drop, Total Energy | 16.3 J @Temperature 22.8 °C |
12.0 ft-lb @Temperature 73.0 °F |
ASTM D3763 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |