Mechanical Properties Metric English Comments
Dart Drop, Total Energy 19.8 - 21.9 J

@Temperature -18.0 - 0.000 °C
14.6 - 16.2 ft-lb

@Temperature -0.400 - 32.0 °F
Average value: 20.8 J Grade Count:1
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Dart Drop, Total Energy 19.8 - 21.9 J

@Thickness 1.85 - 1.85 mm
14.6 - 16.2 ft-lb

@Thickness 0.0728 - 0.0728 in
Average value: 20.8 J Grade Count:1
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..