Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 22.0 J @Temperature -30.0 °C |
16.2 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
Dart Drop, Total Energy | 22.0 J @Temperature 23.0 °C |
16.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
Dart Drop, Total Energy | 22.0 J @Temperature 23.0 °C |
16.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097.. |
|||
Dart Drop, Total Energy | 22.0 J @Temperature -30.0 °C |
16.2 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak, -30°C @ 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |