Mechanical Properties Metric English Comments
Dart Drop, Total Energy 9.99 - 23.5 J

@Temperature -20.0 - -20.0 °C
7.37 - 17.3 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 16.7 J Grade Count:1
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Dart Drop, Total Energy 9.99 - 23.5 J

@Thickness 3.18 - 3.18 mm
7.37 - 17.3 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 16.7 J Grade Count:1
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..