Polymer Property : Dart Drop, Total Energy = 25.1 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 25.1 J

@Thickness 1.85 mm,
Temperature 23.0 °C
18.5 ft-lb

@Thickness 0.0728 in,
Temperature 73.4 °F
ductile, 3.30 m/sec; ASTM D3763
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne