Polymer Property : Dart Drop, Total Energy = 25.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 25.8 J

@Temperature -40.0 °C
19.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin
Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd..