Dart Drop, Total Energy 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D3763
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor..