Mechanical Properties Metric English Comments
Dart Drop, Total Energy 56.5 J

@Thickness 3.20 mm,
Temperature -29.0 °C
41.7 ft-lb

@Thickness 0.126 in,
Temperature -20.2 °F
ASTM D3763
Styron Pulse® B-270 PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 56.5 J

@Thickness 3.20 mm,
Temperature 23.0 °C
41.7 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D3763
Styron Pulse® B-270 PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 56.5 J

@Thickness 3.20 mm,
Temperature 23.0 °C
41.7 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
6.6 m/sec; ASTM D3763
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..