Mechanical Properties Metric English Comments
Dart Drop, Total Energy 63.0 J

@Temperature 23.0 °C
46.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® V2105U PBT
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
Dart Drop, Total Energy 63.0 J

@Temperature 23.0 °C
46.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East)
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
Dart Drop, Total Energy 63.0 J

@Temperature 23.0 °C
46.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific)
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.