Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 93.0 J @Temperature 23.0 °C |
68.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Dart Drop, Total Energy | 93.0 J @Temperature -20.0 °C |
68.6 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Dart Drop, Total Energy | 93.0 J @Temperature 23.0 °C |
68.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Dart Drop, Total Energy | 93.0 J @Temperature -20.0 °C |
68.6 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Dart Drop, Total Energy | 93.0 J @Temperature 23.0 °C |
68.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Dart Drop, Total Energy | 93.0 J @Temperature -20.0 °C |
68.6 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |