Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 10.8 J @Temperature -5.56 °C |
8.00 ft-lb @Temperature 22.0 °F |
ASTM D5420 |
Spartech EP6220 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Gardner Impact | 10.8 J @Temperature -5.56 °C |
8.00 ft-lb @Temperature 22.0 °F |
ASTM D5420 |
Spartech PE4312 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |