Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.0 J @Temperature 23.0 °C |
14.7 ft-lb @Temperature 73.4 °F |
ASTM D3029 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Gardner Impact | 19.9 J @Temperature 23.0 °C |
14.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Medium Impact Copolymer 40% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |