Polymer Property : Gardner Impact = 17.6 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 23.8 J

@Thickness 3.17 mm,
Temperature 22.8 °C
17.6 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
Geometry GC; ASTM D5420
ExxonMobil Exxtral™ MDK310 Performance Polyolefin
Product Description: A medium melt flow rate, 20% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc..