Gardner Impact 4.00 J

@Temperature -29.0 °C
2.95 ft-lb

@Temperature -20.2 °F
6 m/s; ASTM D5420
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene
Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc..
Gardner Impact 4.00 J

@Temperature -40.0 °C
2.95 ft-lb

@Temperature -40.0 °F
ASTM D3029
SABIC Innovative Plastics NORYL EN265 PPE+PS
Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated.