Mechanical Properties Metric English Comments
Gardner Impact 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Valox® 365 PET
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region.
Gardner Impact 37.0 J

@Temperature 23.0 °C
27.3 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Valox® 365 PET
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region.