Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 5.54 J

@Temperature -30.0 °C
4.08 ft-lb

@Temperature -22.0 °F
ASTM D5420
Washington Penn Medium Impact Copolymer 30% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..