Mechanical Properties Metric English Comments
Flexural Modulus 0.0121 GPa

@Temperature 150 °C
1.75 ksi

@Temperature 302 °F
ASTM D790
DuPont Performance Polymers VESPEL TP-8541 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and impact performance in high temperature environmentsInformation provided by DuPont Performance Polymers