Polymer Property : Flexural Modulus = 0.330 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.330 GPa

@Temperature 121 °C
47.9 ksi

@Temperature 250 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers