Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.360 GPa @Temperature 90.0 °C |
52.2 ksi @Temperature 194 °F |
ASTM D790 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |