Polymer Property : Flexural Modulus = 0.500 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.500 GPa

@Temperature 80.0 °C
72.5 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 0.500 GPa

@Temperature 80.0 °C
72.5 ksi

@Temperature 176 °F
Practical Use (Water Absorption 3.5%); ASTM-D790
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 0.500 GPa

@Temperature 80.0 °C
72.5 ksi

@Temperature 176 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 0.500 GPa

@Temperature 65.0 °C
72.5 ksi

@Temperature 149 °F
ASTM D790
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..