Flexural Modulus 0.695 GPa

@Temperature 23.0 °C
101 ksi

@Temperature 73.4 °F
50%RH; ASTM D790
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers