Polymer Property : Flexural Modulus = 1.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 3.5%); ASTM-D790
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.10 GPa

@Temperature 80.0 °C
160 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.10 GPa

@Temperature 100 °C
160 ksi

@Temperature 212 °F
ISO 178
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..