Polymer Property : Flexural Modulus = 108.3 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 108.3 GPa

@Temperature 23.0 °C
15710 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, T2C120 Carbon Tape
Hexcel designation: TXX120-12"-F515; Fiber: Toho® G30/500Information provided by HexCel