Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 123 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 123 GPa

@Temperature 232 °C
17800 ksi

@Temperature 450 °F
1255 Hrs
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel
Flexural Modulus 123 GPa

@Temperature 232 °C
17800 ksi

@Temperature 450 °F
1608 Hrs
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel
Flexural Modulus 123 GPa

@Temperature 23.0 °C
17800 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel
Copyright © lookpolymers.com All Rights Reserved