Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.2 GPa @Temperature 25.0 °C |
1910 ksi @Temperature 77.0 °F |
|
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |
|||
Flexural Modulus | 13.2 GPa @Temperature -40.0 °C |
1910 ksi @Temperature -40.0 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |