Polymer Property : Flexural Modulus = 13200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 90.7 GPa

@Temperature 177 °C
13200 ksi

@Temperature 351 °F
IM7 (12K); [0°, 90°]5s; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form
Fiber: IM7-12KInformation provided by HexCel