Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.367 GPa @Temperature -40.0 °C |
1503.6 ksi @Temperature -40.0 °F |
ISO 178 |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |