Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.5 GPa @Temperature 23.0 °C |
1520 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |