Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.9 GPa

@Temperature 121 °C
2600 ksi

@Temperature 250 °F
Dry; ASTM D790
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi..