Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.0 GPa @Temperature 23.0 °C |
1890 ksi @Temperature 73.4 °F |
ISO 178 |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
Flexural Modulus | 13.0 GPa @Temperature -40.0 °C |
1890 ksi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.25%); ASTM-D790 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 13.0 GPa @Temperature -40.0 °C |
1890 ksi @Temperature -40.0 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 13.0 GPa @Temperature -40.0 °C |
1890 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 13.0 GPa @Temperature 23.0 °C |
1890 ksi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.0%); ASTM-D790 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 13.0 GPa @Temperature 250 °C |
1890 ksi @Temperature 482 °F |
ISO 178 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |