Polymer Property : Flexural Modulus = 19.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 19.9 GPa

@Temperature 23.0 °C
2890 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber
Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal..
Flexural Modulus 19.9 GPa

@Temperature 23.0 °C
2890 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp..