Mechanical Properties Metric English Comments
Flexural Modulus 2.01 GPa

@Temperature -40.0 °C
292 ksi

@Temperature -40.0 °F
ASTM D790
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
Flexural Modulus 2.01 GPa

@Temperature -40.0 °C
292 ksi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..