Polymer Property : Flexural Modulus = 203 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.40 GPa

@Temperature 80.0 °C
203 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.40 GPa

@Temperature 23.0 °C
203 ksi

@Temperature 73.4 °F
ISO 178
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive
Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is ..
Flexural Modulus 1.40 GPa

@Temperature -40.0 °C
203 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..