Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.90 GPa

@Temperature 71.0 °C
276 ksi

@Temperature 160 °F
ASTM-D790
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Flexural Modulus 1.90 GPa

@Temperature 260 °C
276 ksi

@Temperature 500 °F
ASTM D790
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide
Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific..
Flexural Modulus 1.90 GPa

@Temperature 23.0 °C
276 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB