Mechanical Properties Metric English Comments
Flexural Modulus 19.3 GPa

@Temperature 216 °C
2800 ksi

@Temperature 420 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Flexural Modulus 19.3 GPa

@Temperature -53.9 °C
2800 ksi

@Temperature -65.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 19.3 GPa

@Temperature 21.1 °C
2800 ksi

@Temperature 70.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 19.3 GPa

@Temperature 93.3 °C
2800 ksi

@Temperature 200 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 19.3 GPa

@Temperature 23.9 °C
2800 ksi

@Temperature 75.0 °F
Wet (2hr water boil); ASTM D790
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160..
Flexural Modulus 19.3 GPa

@Temperature 121 °C
2800 ksi

@Temperature 250 °F
Wet; ASTM D790
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..
Flexural Modulus 19.3 GPa

@Temperature 23.0 °C
2800 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree..
Flexural Modulus 19.3 GPa

@Thickness 1.57 mm
2800 ksi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..
Flexural Modulus 19.3 GPa

@Temperature 23.0 °C
2800 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..