Mechanical Properties Metric English Comments
Flexural Modulus 24.8 GPa

@Temperature 87.8 °C
3600 ksi

@Temperature 190 °F
Wet (2hr water boil immersion); ASTM D790
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Flexural Modulus 24.8 GPa

@Temperature 71.1 °C
3600 ksi

@Temperature 160 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 24.8 GPa

@Temperature -53.9 °C
3600 ksi

@Temperature -65.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Modulus 24.8 GPa

@Temperature 23.9 °C
3600 ksi

@Temperature 75.0 °F
Dry; 325°F Autoclave Cured; ASTM D790
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Flexural Modulus 24.8 GPa

@Temperature 23.9 °C
3600 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D790
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Flexural Modulus 24.8 GPa

@Temperature 82.2 °C
3600 ksi

@Temperature 180 °F
0° Direction, Wet; ASTM D790
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Flexural Modulus 24.8 GPa

@Temperature 177 °C
3600 ksi

@Temperature 351 °F
Wet condition - 96 hours in boiling H2O
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement
Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel