Polymer Property : Flexural Modulus = 363 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.50 GPa

@Temperature -20.0 °C
363 ksi

@Temperature -4.00 °F
ISO 178
Polykemi AB POLYfill PP HGX500707 Polypropylene, Multifiller
Information provided by Polykemi AB
Flexural Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer  (Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
Flexural Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
ASTM-D790
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Flexural Modulus 2.50 GPa

@Temperature 80.0 °C
363 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.50 GPa

@Temperature 80.0 °C
363 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..